S275J2G3
2017-11-14 15:29:21
We are a professional manufacturer of S275J2G3, we can provide the third party inspection report and datasheet of S275J2G3 as round bar, square bar, flat steel and so on. Please send the inquiry to us if you are if you are interested in S275J2G3. We will serve you with honesty, integrity, and professional. The detail data as below follow:
Steel Grade: S275J2G3| Material No.: 1.0144 | Equal Germany DIN: St44-3N
CHEMICAL COMPOSITION(S275J2G3):
C(%) : 0.18
Si (%): —
Mn(%): 1.5
P(%)≤: 0.035
S(%)≤: 0.035
Other(%) : —
MECHANICAL PROPERTIES (S275J2G3):
Yield Strength|σ0.2/Mpa(≤16mm): 275
Tensile Strength|σb/Mpa(≤3mm): 430~580
Ballistic Temperature(℃): -20/-20
Ballistic|αkv≥(J/cm^2)(10-150mm): 27/27
Test Sample(L/T) : L/T
Extensibility|δ(%)(3-40mm) : 22/20
Remark(S275J2G3):
1, U-->Rimmed Steel, N-->Non-Rimmed Steel,;F-->Full Killed Steel.
2, The ω(P) will be reduced 0.005% per the ω(N) have be increased 0.001%[ω(N)≤0.012%].
3, When the ω(Al) is more than 0.02% or there is strong oxide elements is this steel, then the ω(N) is not correct in this table.
4, L-->Length, T-->Crosswise.
5, The standard of sample for extensibility testing is L0=5.65×S0^1/2.
6, The standard of steel grade and chemical composition is DIN EN 10025(1998)
Introduction structural steel (S275J2G3)
Structural steel is a steel that conforms to a specific strength and formability grade. The formability is expressed as the elongation at the end of the tensile test. Structural steel is generally used for bearing and other purposes. In these uses, the strength of steel is an important design standard.
Most steels used throughout Europe are specified to comply with the European standard EN 10025. However, many national standards also remain in force.
Typical grades are described as 'S275J2' or 'S355K2W'. In these examples, 'S' denotes structural rather than engineering steel; 275 or 355 denotes the yield strength in newtons per square millimetre or the equivalent megapascals; J2 or K2 denotes the materials toughness by reference to Charpy impact test values; and the 'W' denotes weathering steel. Further letters can be used to designate fine grain steel ('N' or 'NL'); quenched and tempered steel ('Q' or 'QL'); and thermomechanically rolled steel ('M' or 'ML').
Application(S275J2G3)
Structural steel is a category of steel used for making construction materials in a variety of shapes. Many structural steel shapes take the form of an elongated beam having a profile of a specific cross section. Structural steel shapes, sizes, chemical composition, mechanical properties such as strengths, storage practices, etc., are regulated by standards in most industrialized countries.
HOT SALE:
SA-675GR70, SA-387GR91, X6NiCrTiMoVB25-15-2, 17-4PH, 15-5PH,
ASTM 630, X3CrNiMo13-4, UNS41500, X10CrNiTi18-10, S17400,
X5CrNiCuNbl6-4, 316Ti, 301A, 303, 304L, 310S, 316L, 317L, 321,
NKA80, DIN 1.4731, DIN 1.4021, DIN 1.4016, DIN 1.4571, DIN 1.4418,
616, 440B, 440C, 431, 430FR, 430F, 430, 422, 416, 410, 405,
ASTM D2, X155CrMoV12-1, ASTM D3, AISI H11, AISI H13
Steel Grade: S275J2G3| Material No.: 1.0144 | Equal Germany DIN: St44-3N
CHEMICAL COMPOSITION(S275J2G3):
C(%) : 0.18
Si (%): —
Mn(%): 1.5
P(%)≤: 0.035
S(%)≤: 0.035
Other(%) : —
MECHANICAL PROPERTIES (S275J2G3):
Yield Strength|σ0.2/Mpa(≤16mm): 275
Tensile Strength|σb/Mpa(≤3mm): 430~580
Ballistic Temperature(℃): -20/-20
Ballistic|αkv≥(J/cm^2)(10-150mm): 27/27
Test Sample(L/T) : L/T
Extensibility|δ(%)(3-40mm) : 22/20
Remark(S275J2G3):
1, U-->Rimmed Steel, N-->Non-Rimmed Steel,;F-->Full Killed Steel.
2, The ω(P) will be reduced 0.005% per the ω(N) have be increased 0.001%[ω(N)≤0.012%].
3, When the ω(Al) is more than 0.02% or there is strong oxide elements is this steel, then the ω(N) is not correct in this table.
4, L-->Length, T-->Crosswise.
5, The standard of sample for extensibility testing is L0=5.65×S0^1/2.
6, The standard of steel grade and chemical composition is DIN EN 10025(1998)
Introduction structural steel (S275J2G3)
Structural steel is a steel that conforms to a specific strength and formability grade. The formability is expressed as the elongation at the end of the tensile test. Structural steel is generally used for bearing and other purposes. In these uses, the strength of steel is an important design standard.
Most steels used throughout Europe are specified to comply with the European standard EN 10025. However, many national standards also remain in force.
Typical grades are described as 'S275J2' or 'S355K2W'. In these examples, 'S' denotes structural rather than engineering steel; 275 or 355 denotes the yield strength in newtons per square millimetre or the equivalent megapascals; J2 or K2 denotes the materials toughness by reference to Charpy impact test values; and the 'W' denotes weathering steel. Further letters can be used to designate fine grain steel ('N' or 'NL'); quenched and tempered steel ('Q' or 'QL'); and thermomechanically rolled steel ('M' or 'ML').
Application(S275J2G3)
Structural steel is a category of steel used for making construction materials in a variety of shapes. Many structural steel shapes take the form of an elongated beam having a profile of a specific cross section. Structural steel shapes, sizes, chemical composition, mechanical properties such as strengths, storage practices, etc., are regulated by standards in most industrialized countries.
HOT SALE:
SA-675GR70, SA-387GR91, X6NiCrTiMoVB25-15-2, 17-4PH, 15-5PH,
ASTM 630, X3CrNiMo13-4, UNS41500, X10CrNiTi18-10, S17400,
X5CrNiCuNbl6-4, 316Ti, 301A, 303, 304L, 310S, 316L, 317L, 321,
NKA80, DIN 1.4731, DIN 1.4021, DIN 1.4016, DIN 1.4571, DIN 1.4418,
616, 440B, 440C, 431, 430FR, 430F, 430, 422, 416, 410, 405,
ASTM D2, X155CrMoV12-1, ASTM D3, AISI H11, AISI H13
The last:
26CrMo7
Next up:
20CrMoV13-5