We are a professional manufacturer of C35C, we can provide the third party inspection report and datasheet of C35C as round bar, square bar, flat steel and so on. Please send the inquiry to us if you are if you are interested in C35C. We will serve you with honesty, integrity, and professional. The detail data as below follow:
Steel Grade: C35C| Material No.: 1.1172
CHEMICAL COMPOSITION(C35C):
C(%) : 0.32~0.39
Si(%) : ≤0.40
Mn(%) : 0.50~0.80
P(%)≤: 0.035
S(%)≤: 0.035
Cr(%) : —
Mo(%) : —
Ni(%) : —
HARDNESS AND HEAT TREATMENT(C35C):
Quench/℃|Water: 840~870
Quench/℃|Oil: 850~880
Temper/℃: 550~660
MECHANICAL PROPERTIES④ (C35C):
Softening Annealing/℃
: 650~700
Tensile Strength(≤100mm)|σb/MPa②③: 590①
Reduction of Area(≤100mm)|ψ(%)②③: 58①
Tensile Strength(≤60mm)|σb/MPa②④: 570
Reduction of Area(≤60mm)|ψ(%)②④: 60
Tensile Strength≥|σb/MPa⑥: 580~730
Yield Strength≥|σs/MPa⑥: 365
Extensibility≥|δ5(%)⑥: 19
Reduction of Area≥|ψ(%)⑥: 45
Ballistic≥|AKV/J①⑥: 41
Remark(C35C):
①, The test sample is according to DVM-V.
②, It is mechanical properties for cold upsetting and cold extruding.
③, It is softening annealing.
④, It is cold-drawing softening annealing.
⑤, The standard is DIN 1654(1989).
⑥, It is mechanical properties after hot working.
Introduction structural steel (C35C)
Structural steel is a steel that conforms to a specific strength and formability grade. The formability is expressed as the elongation at the end of the tensile test. Structural steel is generally used for bearing and other purposes. In these uses, the strength of steel is an important design standard.
Most steels used throughout Europe are specified to comply with the European standard EN 10025. However, many national standards also remain in force.
Typical grades are described as 'S275J2' or 'S355K2W'. In these examples, 'S' denotes structural rather than engineering steel; 275 or 355 denotes the yield strength in newtons per square millimetre or the equivalent megapascals; J2 or K2 denotes the materials toughness by reference to Charpy impact test values; and the 'W' denotes weathering steel. Further letters can be used to designate fine grain steel ('N' or 'NL'); quenched and tempered steel ('Q' or 'QL'); and thermomechanically rolled steel ('M' or 'ML').
Application(C35C)
Structural steel is a category of steel used for making construction materials in a variety of shapes. Many structural steel shapes take the form of an elongated beam having a profile of a specific cross section. Structural steel shapes, sizes, chemical composition, mechanical properties such as strengths, storage practices, etc., are regulated by standards in most industrialized countries.
HOT SALE:
SA-675GR70, SA-387GR91, X6NiCrTiMoVB25-15-2, 17-4PH, 15-5PH,
ASTM 630, X3CrNiMo13-4, UNS41500, X10CrNiTi18-10, S17400,
X5CrNiCuNbl6-4, 316Ti, 301A, 303, 304L, 310S, 316L, 317L, 321,
NKA80, DIN 1.4731, DIN 1.4021, DIN 1.4016, DIN 1.4571, DIN 1.4418,
616, 440B, 440C, 431, 430FR, 430F, 430, 422, 416, 410, 405,
ASTM D2, X155CrMoV12-1, ASTM D3, AISI H11, AISI H13, C35C
Steel Grade: C35C| Material No.: 1.1172
CHEMICAL COMPOSITION(C35C):
C(%) : 0.32~0.39
Si(%) : ≤0.40
Mn(%) : 0.50~0.80
P(%)≤: 0.035
S(%)≤: 0.035
Cr(%) : —
Mo(%) : —
Ni(%) : —
HARDNESS AND HEAT TREATMENT(C35C):
Quench/℃|Water: 840~870
Quench/℃|Oil: 850~880
Temper/℃: 550~660
MECHANICAL PROPERTIES④ (C35C):
Softening Annealing/℃
: 650~700
Tensile Strength(≤100mm)|σb/MPa②③: 590①
Reduction of Area(≤100mm)|ψ(%)②③: 58①
Tensile Strength(≤60mm)|σb/MPa②④: 570
Reduction of Area(≤60mm)|ψ(%)②④: 60
Tensile Strength≥|σb/MPa⑥: 580~730
Yield Strength≥|σs/MPa⑥: 365
Extensibility≥|δ5(%)⑥: 19
Reduction of Area≥|ψ(%)⑥: 45
Ballistic≥|AKV/J①⑥: 41
Remark(C35C):
①, The test sample is according to DVM-V.
②, It is mechanical properties for cold upsetting and cold extruding.
③, It is softening annealing.
④, It is cold-drawing softening annealing.
⑤, The standard is DIN 1654(1989).
⑥, It is mechanical properties after hot working.
Introduction structural steel (C35C)
Structural steel is a steel that conforms to a specific strength and formability grade. The formability is expressed as the elongation at the end of the tensile test. Structural steel is generally used for bearing and other purposes. In these uses, the strength of steel is an important design standard.
Most steels used throughout Europe are specified to comply with the European standard EN 10025. However, many national standards also remain in force.
Typical grades are described as 'S275J2' or 'S355K2W'. In these examples, 'S' denotes structural rather than engineering steel; 275 or 355 denotes the yield strength in newtons per square millimetre or the equivalent megapascals; J2 or K2 denotes the materials toughness by reference to Charpy impact test values; and the 'W' denotes weathering steel. Further letters can be used to designate fine grain steel ('N' or 'NL'); quenched and tempered steel ('Q' or 'QL'); and thermomechanically rolled steel ('M' or 'ML').
Application(C35C)
Structural steel is a category of steel used for making construction materials in a variety of shapes. Many structural steel shapes take the form of an elongated beam having a profile of a specific cross section. Structural steel shapes, sizes, chemical composition, mechanical properties such as strengths, storage practices, etc., are regulated by standards in most industrialized countries.
HOT SALE:
SA-675GR70, SA-387GR91, X6NiCrTiMoVB25-15-2, 17-4PH, 15-5PH,
ASTM 630, X3CrNiMo13-4, UNS41500, X10CrNiTi18-10, S17400,
X5CrNiCuNbl6-4, 316Ti, 301A, 303, 304L, 310S, 316L, 317L, 321,