We are a professional manufacturer of W210 Standard, we can provide the third party inspection report and datasheet of W210 Standard as round bar, square bar, flat steel and so on. Please send the inquiry to us if you are if you are interested in W210 Standard. We will serve you with honesty, integrity, and professional. The detail data as below follow: 
Steel Grade: ASTM W210 Standard
CHEMICAL COMPOSITION(W210 Standard): 
C(%) :         ②
Si(%) :        0.10~0.40
Mn(%) :         0.10~0.40
Cr(%):         0.03
V(%):         0.03
HARDNESS AND HEAT TREATMENT (W210 Standard):
Initial Forging Temperature/℃:         980~1070
Finish Forging Temperature/℃:        820
Annealing/℃:        760~790
Hardness HBS|After Annealing :         159~202
Quenching/℃:        770~840
Quenching Medium:        Brine or Water
Tempering/℃:         150~340
Hardness HBS|After Tempering:         65~50
Remark(W210 Standard): 
①, It will be used this temperature if the ω(C) is between 0.50%~1.25%, it should be used the lower limit temperature if the ω(C) is between 1.25%~1.40%.
②, It will be used 740~760℃ if the ω(C) is between 0.60%~0.90%, it should be used 760~790℃ if the ω(C) is between 0.90%~1.40%.
③, It will be used 790~840℃ if the ω(C) is between 0.60%~0.80%, it should be used 770~840℃ if the ω(C) is between 0.85%~1.05%, it should be used 760~830℃ if the ω(C) is between 1.10%~1.40%.
④, The chemical composition which have parenthesis means Si+Mn+Cr≤0.75%.
⑤, The AISI W108、W109、W110、W112 are same as UNS T72301, the AISI W209、W210 are same as UNS T72302, the AISI W5 is same as UNS T72305.
⑥, The composition of P,S and residual elements is follow: P≤0.025%;S≤0.025%;Cu≤0.20%.
Please find the PDF for W210 Standard  
Introduction Cemented Carbide (W210 Standard)
Cemented carbide is made of refractory metal hard compound and binding metal through powder metallurgy technology made of an alloy material.
Cemented carbide with high hardness, wear resistance, good strength and toughness, heat resistance, corrosion resistance and a series of excellent properties, especially its high hardness and wear resistance, even under the temperature of 500 ℃ is basic remains the same, there are still very high hardness at 1000 ℃.

HOT SALE: 
SA-675GR70, SA-387GR91, X6NiCrTiMoVB25-15-2, 17-4PH, 15-5PH,
ASTM 630, X3CrNiMo13-4, UNS41500, X10CrNiTi18-10, S17400,
X5CrNiCuNbl6-4, 316Ti, 301A, 303, 304L, 310S, 316L, 317L, 321,
NKA80, DIN 1.4731, DIN 1.4021, DIN 1.4016, DIN 1.4571, DIN 1.4418,
616, 440B, 440C, 431, 430FR, 430F, 430, 422, 416, 410, 405,
ASTM D2, X155CrMoV12-1, ASTM D3, AISI H11, AISI H13,  W210 Standard

Special Steel, Tapping Machine, Cold Heading Machine Supplier in China-Copy Right By Hacer Technology